Shanxi anthracite was subjected to oxygen-oxidation at 250°C in all aqueous solution of potassium hydroxide to produce solid benzene polycarboxylic acid (BPCA), and then the BPCA were selectively decarboxylated in the mixed medium of concentrated H2SO4 and KHSO4 to produce crude pyromellitic acid (PA). Pure PA was obtained by solvent recrystallization method, and the best solvent was 2-pentanone. Pure pyromellitic anhydride (PMDA) was gotton by heating pure pyromellitic acid in vacuum chamber at 260°C for 3 h. The remaining BPCA which through 2-pentanone recrystallization was isomerizated with consistent temperature at 420°C for 2 h. Appropriation pH of BPCA, initial pressure of carbon dioxide and cadmium carbonate catalyst were provided to produce crude terephthalic acid (TPA). Pure TPA was obtained by washing and drying the crude TPA precipitation.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.