Abstract
This study used alumina fine as main raw materials to prepare the porous ceramic separation membrane supports. The effects of different the sintering temperature and holding time on ceramic separation membrane supports are studied, and the TG/DSC curves of raw materials powder are analyzed by the preparation process. The results show that sintering temperature 1200°C, holding time 6 h, pore-forming agent more than 20%, prepared the uniform pore size distribution, porosity, accord with more than 50% of porous ceramics water demand separation membrane supports.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.