Abstract

Poly(3,4-ethylenedioxythiophene) (PEDOT) was fabricated via vapor-phase polymerization (VPP) of the monomer 3,4-ethylenedioxythiophene (EDOT) with FeCl3·6H2O melt as the oxidant at the EDOT vapor–FeCl3·6H2O melt interface. Highly doped VPP-PEDOT films were formed on the oxidant melt surfaces. The morphological changes and decrease in the doping level at the VPP-PEDOT film surface were attributed to slower oxidant transport up to the surface during VPP. The doping level of VPP-PEDOT was higher when the oxidant melt was used compared to when the oxidant thin film was employed, and the maximum doping level was twice of that obtained in our previous work.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.