The preparation of nickel powders by the ultrasonic spray pyrolysis of Ni(HCOO)2 was studied. Phase‐pure nickel powder was obtained at as low as 350°C. HCOOH was a reducing source for nickel formation. Moreover, metallic nickel was obtained at a residence time as short as 0.1 s at 600°C. A broad range of particle morphologies, which included agglomerated nanoparticles, nonagglomerated submicrometer particles, hollow particles, and spherical dense particles, were obtained from Ni(HCOO)2 pyrolysis and were shown to depend on the precursor solution and the operating condition.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.