Abstract

This study presents different fuels (Glycine and Urea) that can be used to synthesize nanocrystalline forsterite by the sol-gel combustion method. The weight change of precursor during thermal treatment was studied by thermo-gravimetric analysis (TGA). Pure forsterite was characterized by heating microscopy, Fourier transform infrared spectroscopy, X-ray Diffraction, Brunauer-Emmett-Teller, Scanning Electron Microscopy, and Energy dispersive X-ray spectroscopy. The HAP (hydroxyapatite) deposition ability, degradation and dissolution behaviour of forsterite was examined in simulated body fluid (SBF). The combusted forsterite precursor showed distinct thermal behaviour for each fuel when analyzed by heating microscopy. BET analysis showed that the particle size of forsterite synthesized using glycine was 28nm, specific surface area 65.11m2/g and average pore diameter 16.4nm while using urea 1.951μm, 0.939m2/g, and 30.5nm are the respective parameters. The dissolution of forsterite pointed to the consumption of Ca and P ions from SBF, the negligible release of Si ion into the SBF and these ionic interactions with SBF can be altered as per the material properties. The forsterite showed good antibacterial activity against S. aureus but lower activity against E. coli. The bactericidal activity of forsterite indicated that it can be used to inhibit biofilm formation in dental, bone implants and bacterial infection during surgical operations.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call