Abstract

The preparation of lithium niobate powder, LiNbO3, using an organic niobium salt and lithium nitrate in a buffer solution of oxalic acid and ammonium oxalate has been investigated. After the evaporation of this starting solution a precursor is obtained, which upon heat treatment, yields LiNbO3. A chemical formula for this precursor is proposed, based on IR and thermal analysis data. The thermal evolution of the precursor powder, to the point of the formation of the LiNbO3 phase, was followed by means of thermal analysis, IR spectroscopy and powder X-ray diffraction (XRD). The results indicate that total crystallization occurs after a 550 °C heat treatment, showing that single-phase LiNbO3 powder, with a crystallite mean size of 88 nm, can be prepared at low processing temperatures.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.