BaCe0.7Zr0.1Y0.16Zn0.04O3-δ (BCZYZ) ceramic slurry has been prepared with different solid loading and the maximum solid loading of the slurry has been predicted as 25 vol.% using the Krieger-Dougherty equation. The slurry with the maximum solid loading has been formulated and applied as an electrolyte on porous NiO/BCZYZ tubular supports by the dip-coating method. Cells sintered at 1500°C for 10h have been characterised by Scanning Electron Microscopy (SEM) analysis. The 30μ thick, very dense electrolyte layer has successfully been achieved with some closed pores.