Abstract

Novel visible-light-driven graphitic carbon nitride (g-C3N4)/WO3 composite photocatalysts were prepared, and the acetaldehyde (CH3CHO) degradation activity of these composites was evaluated. The prepared g-C3N4/WO3 composites were characterized by X-ray diffraction (XRD), Fourier transform infrared spectroscopy (FT-IR), scanning electron microscopy (SEM), transmission electron microscopy (TEM), ultraviolet–visible diffuse reflection spectroscopy (UV–vis), and the N2 gas adsorption Brunauer–Emmett–Teller (BET) method (N2-BET). The WO3 particles, which were 100–300nm in size, were in direct contact with the g-C3N4 sheet surface. The optical band gap and specific surface area of the g-C3N4/WO3 composites were in the range of 2.65–2.75eV and 4–7m2/g, respectively. The g-C3N4/WO3 composites exhibited higher activity for the photodegradation of CH3CHO under visible light irradiation compared to g-C3N4. The optimal WO3 content for the CH3CHO photodegradation activity of the heterojunction structures was determined. The synergistic effect of g-C3N4 and WO3 was considered to lead to improved photogenerated carrier separation. A possible degradation mechanism of CH3CHO over the g-C3N4/WO3 composite photocatalyst under visible light irradiation was proposed. These results should usefully expand applications of g-C3N4 as a visible-light-driven photocatalyst.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.