Abstract

The present investigation reports the preparation of freestanding nanocrystalline Zn by combined mechanical milling at cryogenic and room temperatures. The cryomilling is used as an effective means of rapid fracturing. The detailed scanning electron microscopy and transmission electron microscopy observations indicate that the minimum crystallite size is 6 ± 2 nm after 3 hours of cryomilling. The crystallite size increases to 30 ± 2 nm after 3 hours of room temperature milling of the cryomilled powder due to deformation-induced sintering. Detailed theoretical analysis allows us to obtain a diagram of size of the nanoparticles formed vs temperature to explain the experimental findings.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.