Abstract

• Isolation of Kraft and organosolv lignin from Kenaf core. • Higher molecular weight of Kraft lignin was probably due to the more severe reaction condition. • Preparation of lignin phenol formaldehyde (LPF) wood adhesive. • 50% KLPF adhesive shows higher tensile strength than that of commercial PF.