Abstract

A one-pot reaction of zirconium oxychloride octahydrate (ZOC) with ethyl acetoacetate (Hetac) in the presence of triethylamine was investigated. The reaction was carried out in molar ratios of Hetac/ZOC=1.0, 1.5, 2.0 to give highly viscous solutions with good spinnability and stability to self-condensation. Polyzirconoxanes (PZOs) were isolated as white powders by reprecipitation of the solutions with tetrahydrofuron (THF)-hexane that were soluble in acetone, methanol and THF. The molecular weight of PZO was Mn=1000–2000, and was dependent on the molar ratio and the reaction time. Dry spinning of the solution (Hetac/ZOC=1.5) containing 3mol% tris(acetylacetonato)yttrium [Y(acac)3] gave continuous precursor fibres (3.0Y–PZO). Yttria stabilized zirconia fibres of 12–18 μm diameter with a tensile strength of 1.4GPa were obtained by heat treatment of the 3.0Y–PZO at 1100 or 1200 °C. The fibre consisted of submicrometre-sized particles of tetragonal crystallites. © 1998 Chapman & Hall

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.