In the present study, a causticization method combined with alkaline leaching and purification process was used to treat with lead refining slag. In the alkaline leaching process, the effects of alkaline concentration, temperature, liquid to solid ratio, leaching time, and agitating speed were investigated, and the optimized leaching conditions were established: 2 mol/L of NaOH concentration, 2 h of leaching time, 85 °C of temperature, 6 mL/g of liquid-to-solid ratio, 800 r/min of agitating speed. Under these conditions, the leaching rate of Sn reached 92% while the leaching rate of Pb was about 29%. After a purification process, the concentration of lead in the leachate was reduced to 0.0001 g/L. Finally, high-purity calcium stannate (CaSnO3·3H2O) was obtained from the purified solution by the causticization process under the conditions: 5 g of CaO dosage (per 200 mL solution), 85 °C of temperature, 2 h of time and 800 r/min of agitating speed. The precipitation rate of Sn was as high as 99.22%.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.