Abstract

Al-Sc master alloy is prepared by aluminothermic reaction with a kind of special molten salt under the normal atmospheric condition. To achieve larger Sc recovery rate, the composition and pretreatment of the molten salt are studied. The optimum molten salt is obtained by melting together Sc2O3, NaF, KCl, NaCl, ScF3 and Na3AlF6 mixture under a mass ratio of 3:5:10:10:2:30, followed by solidifying and crushing. The pretreated salt is added to the Aluminum melt with a mass ratio of 60:100 to prepare Al-Sc master alloy. When the residue of molten salt is reused for three times, the Sc recovery rate can reach 91%. The structure and composition of the residue are examined using X-ray diffraction (XRD) analyzer and differential scanning calorimetry (DSC) analyzer. Based on the analysis of the residue, mechanism of the aluminothermic reaction to achieve larger Sc recovery rate with this special molten salt is discussed.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.