Fly ash from waste incineration and waste poplar bark from furniture manufacturing are domestic wastes. In this study, fly ash and poplar bark were used as raw materials to prepare activated carbon via carbonization, steam activation and reagent modification. The effects of the raw material mixing ratio, carbonization temperature, activator concentration and modifier concentration on the physicochemical properties of the semi-coke and activated carbon were investigated through experiments. The experiment showed that when the carbonization temperature was 300 °C, the steam concentration was 20%, the mixing ratio of the poplar bark and fly ash (B:F) was 5:1, and the modifier was 6% K2CO3 reagent and 9% CaCl2. The prepared activated carbon had a better yield, specific surface area and pore structure, and had an abundant surface functional group structure. This paper points out the direction for the industrial directional production of activated carbon adsorbents with excellent physical and chemical properties, which has practical significance.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call