Abstract

(1−x)(Bi,K)TiO3−xCaTiO3 epitaxial films with x = 0–1.0 were grown on (100) c SrRuO3//(100)SrTiO3 substrates by the hydrothermal method. The film composition region can be divided into three in view of its crystal structure. The films in the range of x = 0–0.12 (Region 1) and 0.60–1.0 (Region 3) consisted of a single phase and their lattice parameters changed with the x value. This suggests the formation of a solid solution. On the other hand, two phases coexisted in the intermediate range of x = 0.18–0.43 (Region 2). The ferroelectricity and the effective transverse piezoelectric coefficient, effective d 33, were observed for the films in Regions 1 and 2. The slope difference of P r and the effective d 33 against x can be explained by the change in the tetragonality of the films with x in Region 1 and the volume fraction of the ferroelectric phase in Region 2.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.