"The polymer blend of Chitosan: polyvinyl alcohol (PVA) (1:1) weight percent and hydroxyethyl cellulose (HEC) (0.5%) was prepared. The profile of the sample and its properties were measured by Fourier transfer Infrared spectroscopy (FTIR). The Scanning Electron Microscopy (FESEM) was used to describe the morphology of the polymer blend with two magnifications without any ratio of 4- (2-Pyridylazo) resorcinol monosodium salt hydrate and with 0.15 % of a 4-(2-Pyridylazo) resorcinol monosodium salt hydrate. The mechanical properties were demonstrated and characterized by Elongation and Young modulus. The polymer blend was incorporated with different weight ratios of 4-(2-Pyridylazo) of resorcinol monosodium salt hydrate, (0.03, 0.05, 0.07, 0.09, 0.15) gm of weight %. The current-voltage (I-V) characterization of prepared thin films showed ohmic behavior and the electrical conductivity was improved by increasing the ratio of dopant that leads all samples to reflect a semiconductor behavior.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.