Abstract

Co-γFe2O3perpendicular magnetic recording media were preparedby the CoO-Fe3O4single-1ayer deposition method, which is more suitable for mass production than the CoO/ Fe3O4 multilayer deposition method. Moderately <100>-oriented Co-γFe2O3media with intermediate perpendicular anisotropy (Ku=6.0 × 105erg/cm3) were prepared with a wide range of film thicknesses and oxygen partial pressure used in deposition of NiO underlayers. These media showed a superior high-density recording performance comparable to that of highly <100>-oriented Co-γFe2O3 media with large perpendicular anisotropy (Ku=1.4 × 106 erg/cm3). It is surmised that the superior performance of these media was supported by the longitudinal magnetic component as well as the perpendicular one.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.