Abstract
The sisal cellulose was dissolved in ILs under optimal conditions of 150°C and 400W. The structure of sisal cellulose was changed from cellulose I to cellulose II, accompanied with the decrease of crystallinity through XRD, FT-IR analysis. According to the result of GPC, molecular weight distribution became more uniformly and narrow. This is because intra-and inter-hydrogen bond existed in cellulose were destroyed during the dissolution process in ILs. And the regenerated cellulose possessed better properties than the former, which could broaden the application fields of natural cellulose.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.