Abstract

Os–Ir–Al alloy was fabricated by powder metallurgy technique. IrAl and OsIr interalloys were synthesized to reduce the Al evaporation and ensure the composition of the ternary alloy. Analysis on microstructures shows that each component is distributed homogeneously, and the green density reaches 94.9 %. Ba–W cathodes with Os–Ir–Al alloy magnetic sputtered on the tips are prepared and directly current density tests are carried out on these cathodes. It is found that at 1,050 °C, the average zero field emission density of the cathode reaches up to 20 A·cm−2. The improvements of cathodic current density and stability may indicate the prosperous application of Os–Ir–Al alloy on cathode.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.