Silica alcogels were prepared by hydrolysis with hydrochloric acid and condensation with NH4OH of ethanol diluted tetraethylorthosilicate (TEOS) precursor and trimethylchlorosilane and hexane as surface modifying agent. The physical properties such as density, appearance, hydrophobicity, surface area, pore size distribution and thermal stability were measured. It was found that the physical and hydrophobic properties of the silica aerogels depend on the TMCS/hexane (V) volume ratio. The density decreased with increase ofV, and the aerogels are more hydrophobic asV=3%. The aerogels were thermally stable up to a temperature of 350 °C, and the aerogel prepared has a high surface area and large pore volume.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.