Abstract

Glutaraldehyde cross-linked silk sericin films were successfully prepared. FTIR was applied to characterize the chemical structure of films. Compared to pure silk sericin, cross-linked silk sericin film with 3% glutaraldehyde was found a new peak at 1620 cm-1 and the peak intensity of cross-linked film decreased markedly, which indicating cross-linking reaction has been occurred. Thermal and swelling behavior of cross-linked films was investigated. The cross-linking reaction increased the thermal decomposition temperature. The swelling ratio of glutaraldehyde cross-linked silk sericin films went up with increasing glutaralehyde loading to 3wt%.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.