Abstract

A series of cyano-containing polyimides were synthesized from 2,6-bis(4-amino- phenoxy)benzonitrile and some aromatic dianhydride monomers by solution polycondensation. The poly(amic acid) films could be obtained by solution-cast from N-methyl-2-pyrrolidinone solutions and thermally converted into tough polyimide films. Structure and physical properties of thin films of those polyimides were measured by FTIR, TGA, dynamic mechanical analysis and LCR hitester et al. Results showed that the polyimides prepared from 2,6-bis(4-aminophenoxy)- benzonitrile and 2,2-bis[4-(3,4-dicarboxyphenoxy)phenyl]propane dianhydride or 4,4’-(hexafluoropropylidene)diphthalic anhydride exhibited more excellent energy-damping characteristic and excellent solubility in NMP, DMF, DMAc, DMSO, THF and CHCl3, whereas the polyimides from 2,6-bis(4-aminophenoxy)benzonitrile and 3,3’,4,4’-biphenyltetracarboxylic dianhydride or Pyromellitic dianhydride were insoluble in polar and nonpolar organic solvents. All polyimides indicated higher glass transition temperatures, excellent thermal stability and tensile properties. Incorporating a nitrile group into the polyimide backbone would enhance the dielectric constant of the polyimide films.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.