Abstract
In this study, 3-Aminopropyltriethoxysilane (KH550) with polar amino groups is applied to modify the surface of Barium titanate (BaTiO3) particles. When volume fraction of BaTiO3 further increases to 50 vol%, the dielectric constant and loss of HDPE control increase from 2.5 and 0.02 to 18.5 and 0.10 at 10 MHz, respectively, with the volume resistivity of HDPE control decreasing from 3.6 × 1013 Ω m to 3.5 × 1011 Ω m. The increased amount of modified BaTiO3 can increase the flexural strength and modulus HDPE composites from 8 and 90 MPa to 14 and 780 MPa, respectively. However, the increase of modified BaTiO3 can restrict mobility of HDPE chains and decrease the crystallinity of HDPE composites.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Journal of Materials Science: Materials in Electronics
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.