Washcoat deposited on ceramic honeycomb was prepared using pseudoboehmite, the CeO 2–ZrO 2–La 2O 3 solid solution, pore enlarger and other additives. The microstructures and surface performances of washcoat/honeycomb were investigated by SEM, BET surface area, XRD, ultrasonic vibration and hot shock simulation. The results show that the performance and loading of washcoat are affected obviously by the properties of slurry gel, such as the apparent viscosity, solid content, particle size and its distribution. When the apparent viscosity of slurry is lower, the gel with a narrow particle size distribution and finer particles can be obtained, with which the coating having an excellent performance can be prepared. Adding a small quantity of the CeO 2–ZrO 2–La 2O 3 solid solution can promote the thermal stability of washcoat, such as, after calcined at 1000 °C for 5 h the sample exhibits mainly the γ-Al 2O 3 phases and the θ-Al 2O 3 α-Al 2O 3 and κ-Al 2O 3 phases have not been detected in the XRD spectra. It is found also that the washcoat prepared has excellent properties of the vibration-resistant, heat-resistant and its BET surface area reaches 50 m 2/g.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.