Abstract

The copper nanoparticles of average size of 10 nm have been prepared by the sputtering method and characterized through atomic force microscopy (AFM), X-ray diffraction (XRD) and transmission electron microscopy (TEM). The pool boiling heat transfer characteristics of 0.25%, 0.5% and 1.0% by weight concentrations of copper nanoparticles has been studied. Different copper based nanofluids were prepared in both, distilled water and distilled water with 9.0 wt% of sodium lauryl sulphate anionic surfactant (SDS). The pool boiling heat transfer data were acquired for the boiling of nanofluids over a 30 mm square and 0.44 mm thick stainless steel plate heater. The experimental results show that for the critical heat flux of pure water is 80% higher than that of water–surfactant fluid. Also, it was found that the critical heat flux for 0.25%, 0.5% and 1.0% concentrations of copper nanoparticles in copper–water nanofluids are 25%, 40% and 48% higher than that of pure water. But in the case of copper–water with surfactant nanofluids comparing with pure water, the CHF decreases to 75%, 68%, and 62% for respective concentrations of copper nanoparticles. The heat transfer coefficient decreases with increase of nanoparticles concentration in both water–copper and water–copper with surfactant nanofluids.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.