Abstract

Exfoliated graphite with large expanding volume (EV) was prepared by two-step intercalation, in which the mixture of nitric acid and phosphoric acid, and that of nitric acid and acetic acid were employed as intercalating agent step by step, and potassium permanganate was used as oxidant. Its preparation conditions were optimized by orthogonal experiment and parallel experiment, and its microstructure was analyzed by scanning electron microscope. The results show that the optimal preparation conditions for the first step intercalation are as follows: the mass-volume ratio of natural graphite (NG) to mixed acid is 1: 4, the volume ratio of nitric acid to phosphoric acid is 1: 2, the mass ratio of NG to potassium permanganate is 1: 0.2, and the reaction temperature is 20~30°C for 40~60 minutes. Those for the second step intercalation are as follows: the mass-volume ratio of acidized graphite (AG) to acetic acid is 1: 5, the mass-volume ratio of AG to nitric acid is 1: 1.5, the mass ratio of AG to potassium permanganate is 1: 0.15, and the reaction temperature is 20~30°C for 40~60 minutes, the EV is 450ml/g under the conditions listed above. The interlayers of graphite are fully opened and become a worm-like fluffy rope.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.