In this study, (SBA-15)–Eu 2O 3 host-guest composites have been prepared with SBA-15 mesoporous sieve as host and Eu 2O 3 as guest via the solid-phase ultrasonic method and liquid-phase medium ultrasonic method. The host–guest composite materials showed the properties of luminescence. Four excitation peaks appeared in the excitation spectra of the samples. The excitation peaks are located at 397, 415, 466, 537 nm; 392, 408, 464, 532 nm and 393, 406, 465, 533 nm for the nano-Eu 2O 3, the liquid-phase medium ultrasonic method (LPMUM) and the solid-phase ultrasonic method (SPUM) samples, respectively. SBA-15 has the well-ordered hexagonal arrays of mesopores, which makes centrosymmetry of Eu 3+ higher in the prepared (SBA-15)–Eu 2O 3 samples. The intensity of 5D 0→ 7F 1 transition strengthens, and the intensity of 5D 0→ 7F 2 transition weakens.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.