Abstract
A gradient NiCoCrAlYSiB coating was prepared on a Ni-base superalloy using arc ion plating (AIP) and subsequent gaseous phase aluminisation techniques. Hot corrosion of normal NiCoCrAlYSiB and the gradient coating in pure Na 2SO 4 and Na 2SO 4/NaCl (75:25, wt./wt.) salts was performed at 900 °C in static air. The corrosion results indicated an enhanced corrosion resistance to both salts for the gradient NiCoCrAlYSiB coating, which the improved performance of it should be attributed to the β aluminide ‘‘pool” at the surface layer. By partially sacrificing Al 2O 3 (i.e. Al), the gradient NiCoCrAlYSiB coating specimen behaved excellently in the two kinds of salts. The grain growth during the gaseous phase aluminisation and the corrosion mechanism, including the role NaCl played in the mixture salt corrosion, are discussed.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.