Abstract
oriented 0.91Bi1/2Na1/2TiO3–0.06BaTiO3–0.03(Na,K)NbO3 (BNT–BT–KNN) lead-free piezoceramics were fabricated by templated grain growth method. A high grain orientation degree (Lotgering factor F is 83 %) was achieved with 5 wt% Bi1/2Na1/2TiO3 (BNT) template content and a maximum strain value of 0.226 % was observed, which was 48.7 % higher than that of randomly oriented samples. However, too much BNT template will result in composition deviation from morphotropic phase boundary of BNT–BT–KNN system and disruption of the non-polar phase at zero electric field. All textured samples with 1–10 wt% template addition showed enhanced strain and large signal piezoelectric coefficient $$d_{33}^{*}$$ without disrupting the non-polar phase at zero electric field. The enhanced electric-field-induced strain of the textured sample was primarily attributed to the facilitated phase-transition, which formed a long-range ferroelectric order along the direction.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Journal of Materials Science: Materials in Electronics
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.