Abstract

This paper investigates the preparation and electrospinning of acidified-oxidized potato starch. In this article, acidified-oxidized potato starch was prepared by adding ammonium persulfate as an oxidizing agent and hydrochloric acid as a catalyst. The effect of reaction time, temperature, the concentration of hydrochloric acid and the content of ammonium persulfate on the viscosity and content of carboxyl were discussed. The optimum reaction conditions were as follows: 1.5 hours ,50°C, 0.5mol/l HCl, 2.5% (NH4)2S2O8. And then, the acidified-oxidized potato starch prepared at the optimum condition was dissolved in dimethyl sulfoxide (DMSO) to be electrospinned by contrast to native starch. Electrospinning of 5wt%-21wt% of modified starch in DMSO produced beads, beaded fibers, and smooth fibers, depending on the concentration range. Smooth fibers were observed until the concentration reached 19wt%, while native starch was 5wt%.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.