MgAl 2O 4 was prepared by cocrystallizing and decomposing Al(NO 3) 3.9H 2O and Mg(NO 3) 2.6H 2O mixture. The crystallite growth of the resulting powder was studied in the temperature range 500 – 1000 °C. It was found that the equation governing the process is D 2 – D 2 0 = KT. Two activation energies for crystallite growth were obtained, 22 kcal and 44 kcal for the temperature ranges 500 – 785 °C and 785 – 1000 °C respectively. It was noted that rapid increase in crystallite size occurred on soaking at a temperature > 800 °C.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.