Abstract

Zeolite X films have been prepared utilizing pulsed-laser deposition onto TiN-coated silicon wafers and porous stainless steel disks. Laser ablation of zeolite X onto TiN-coated silicon wafers followed by a hydrothermal treatment resulted in partially oriented, crystalline NaX membranes. Hydrothermal treatment of laser-deposited films on stainless steel mesh produced a coated wire mesh with a ∼3-μm-thick zeolite X film. Hydrothermal treatment of the laser-deposited films on 0.5 μm diameter pore stainless steel frits resulted in a densely packed non-continuous film.