Abstract

ABSTRACTAn ITO film on an SiO2 substrate was prepared from spin-coated nano-particles using a simple thermal process and photo irradiation process. The effects of the excimer lamp and excimer laser on the resistivity of the film were investigated. When the film is 40 nm thick, the combined two-step irradiation by an excimer lamp and laser in N2 is effective for the preparation of the ITO film with a lower resistivity. Using the two-step irradiation and one-step KrF irradiation in N2 at room temperature, the resistivity of the ITO film was 5.94×10−4Ωcm. On the other hand, when using the thermal process, the resistivity of the film sintered at 500 °C in N2 was 4.10×10−3Ωcm. The differences in resistivity are discussed on the basis of the microstructure using SEM, XRD and Hall measurements.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.