In this paper, the nonmetallic Si[Formula: see text]-doped modified lanthanum aluminate (LaAlO3) solid electrolyte for the first time, which has particular scientific significance, and LaAl[Formula: see text][Formula: see text]Si[Formula: see text]O[Formula: see text][Formula: see text] material was successfully prepared by the sol–gel method. LaAl[Formula: see text]Si[Formula: see text]O[Formula: see text] is a ceramic material sintered at 1100[Formula: see text]C for 2 h in an air atmosphere. The surface microstructure and electrochemical properties of the samples were tested by multiple characterization methods. The results show that the LaAl[Formula: see text]Si[Formula: see text]O[Formula: see text] has good sintering activity, high crystallinity, and a grain radius of approximately 25 nm. At 800[Formula: see text]C, the ionic conductivity is above 1.05E− 04 S⋅cm[Formula: see text] and the activation energy is lower than 1.19 eV.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.