Abstract

This paper aims at studying the porous cordierite ceramics prepared by using the non-stochiometric cordierite composition formulation (2.8MgO.1.5Al2O3.5SiO2) by PU sponge impregnated method. The ceramic suspension were prepared with non-stoichiometric formulation of cordierite and sintered at 1250 °C, 1275 °C, 1285 °C, 1300 °C and 1325 °C. The phase transformation of non-stochiometric formulation cordierite was investigated by XRD. This paper also aims to compare the effect of linear shrinkage, porosity and density of 20 wt.% PEG treated PU sponge with untreated PU sponge respectively corresponding to different pore content (100 ppi, 80 ppi, 60 ppi, and 40 ppi). The pore structure was analyzed by SEM.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.