Abstract

In order to produce magnetic microparticles (agglomerates), magnetite (Fe 3O 4) particles were synthesized using coprecipitation of FeSO 4·7H 2O and FeCl 3·6H 2O with the presence of poly(methacrylic acid) (PMAA) in aqueous solution.. Transmission electron microscopy (TEM), X-ray diffraction, and vibrating sample magnetometry (VSM) methods were used to characterize the PMAA coated superparamagnetic agglomerates. The influences of various processing parameters such as the process temperature, PMAA content, and the addition of surfactant on the agglomerate size and size distribution of produced magnetic microparticles were investigated. The particle size and size distribution characteristics, (the volume weighted mean size ( D[4,3], surface weighted mean size D[3,2], the geometric standard deviation, and span value) of the magnetic agglomerates were determined using the laser diffraction technique. The PMAA coated magnetic agglomerates with surface weighted mean sizes ranging from 1.5 to 3 μm were produced successfully.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.