Abstract
Mesoporous anatase TiO 2 was prepared for photocatalysis from TiOSO 4 solution. The samples were undoped or doped with chromium. The diffuse reflectance spectra of the samples and the morphology of the TiO 2 particles exhibited strong dependency on the preparation conditions. The mesoporous samples showed good photoactivity upon degradation of acetaldehyde in the visible range (>400 nm) and on degradation of methylene blue in aqueous solution in the UV range (366 nm). The catalyst activity demonstrated strong dependency on crystal size, on particle morphology and porosity, and on doping. Samples heated at 473 K were the most active in the gaseous phase and samples heated at 673 K in the aqueous phase. The pore size of the samples increased upon heating. The chromium-doped samples maintained activity at longer wavelengths (>420 nm) than the undoped samples.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.