Abstract

Grain-oriented Barium titanate (BaTiO3) ceramics were prepared using an electrophoresis deposition (EPD) method under high magnetic field of 12 T and sintering at 1350 °C. It was found that BT03 and BTKK nanoparticles were necessary to synthesize the grain-oriented BT ceramics. The grain orientation was correlated with particles size and c/a ratio of lattice constants. The reason why the grain-oriented BT ceramics using the BT03 and BTKK were prepared was having the large values of the particles size and the c/a ration of lattice constants.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.