Fe3O4 magnetic nanoparticles being used as seeding materials, Ag+ ions on the Fe3O4 magnetic nanoparticles reduced to the metal form by tartaric acid using heated treatment. Thus, Fe3O4/Ag composite core-shell magnetic nanoparticles were synthesized. The products were characterized by transmission electron microscope (TEM) and x-ray diffraction (XRD). Both TEM and XRD results showed that the Ag nanoparticles were well distributed on the surface of Fe3O4 magnetic nanoparticles. The size for Fe3O4/Ag composite magnetic nanoparticles which were spherical shape was ≃40 nm. Furthermore, the magnetic properties of samples were characterized on a vibrating sample magnetometer. Under optimal conditions, Fe3O4/Ag composite nanoparticles showed higher magnetism than pure Fe3O4 nanoparticles.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.