Abstract

SUMMARYThe present work pertains to the study of electroless Ni-P and Ni-P-Si3N4 composite coatings. The deposits are obtained from a proprietary high phosphorus electroless nickel plating bath, comprising nickel sulphate, sodium hypophosphite, complexing agents and stabilizers. The maximum weight percent of Si3N4 incorporated in the electroless deposit is obtained at a concentration of 10 g/l in the bath. The electroless Ni-P deposits having 0%, 2.01%, 5.81% and 8.10% of Si3N4, respectively, obtained from baths containing 0, 2, 5 and 10 g/l of Si3N4, are characterized by optical microscopy, XRD and TEM. Hardness is found to increase with the incorporation of Si3N4 at all heat treatment temperatures studied. Also hardness increases with an increase in weight percent of Si3N4 incorporated in the deposit. The analyses of the composite coatings by XRD and TEM reveal that the inclusion of Si3N4 particles does not change the amorphous nature of the Ni-P matrix.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.