Abstract
The effect of dysprosium and strontium on the total ionic conductivity of ceria in the system Ce1–xDyx–ySryO2–δ was studied. In this system, few compositions were prepared with x=0.15, y=0.015, 0.03 and 0.045 by modified sol–gel process using maltose and pectin as organic precursors. Rietveld refinement of XRD patterns confirms the cubic structure with space group. SEM images show relatively uniform grains with clean and distinct grain boundaries. Four probe AC impedance measurements were carried out to evaluate the total ionic conductivity in the temperature range of 150–500 °C and frequency range of 40 Hz–1 MHz. The composition Ce0.85Dy0.12Sr0.03O2–δ shows higher electrical conductivity than single-doped ceria samples.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Transactions of Nonferrous Metals Society of China
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.