Abstract

Anglicizing the superalloy mechanical and cutting characteristics, and according to the oil-stone grinding characteristics, choose the current commonly abrasives in the domestic. Processing performance test of inconel 718 deep-hole honing is carried out. The comparison test results show that the grinding performance of ceramic corundum is better than other oilstones at test condition. Grinding characteristics of ceramic corundum is carried on, study show that the size of ceramic alumina grits range from 0.067 to 0.005 μm, The grinding passivated tiny grains of ceramic corundum oil-stone broken and fall off timely, which is beneficial to oil-stones, self-sharpness. The excellent performance of ceramic corundumcan self-sharpening can improves the efficiency of honing effectively.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.