Being inspired by nature, a series of experiments was carried out to deposit a calcium oxalate layer on the surface of the stone by the reaction between carbonate rock and oxalate salt. To increase the anti-dissolution properties of the calcium oxalate layer, the use of mixed oxalate solution has been proposed in the literature by two main routes: (1) adding acid agent to ammonium oxalate, which has the advantage of changing the particle structure and reducing layer porosity, and (2) using neutral methyl oxalate solution, which has the advantage of surface coverage due to slowly hydrolysis. In this study, we investigated the sequential application of ammonium oxalate, methyl oxalate, neutral mixed, and calcium acetate acid mixed solution. With this method, calcium carbonate and calcium oxalate solution can react inside the stone to reinforce it. The protective film’s coverage area can then be increased using dimethyl oxalate neutral mixed solution, and the crystal morphology can be modified with calcium oxalate acid mixed solution. The anti-dissolution properties of the coating were investigated using both a custom-designed apparatus and a selective outdoor environment. The coating displayed good acid resistance properties at pH 2–4. After one year of exposure, the coating is firmly bonded with the stone.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.