Abstract

The bioactivity of glass ceramics with different amount of fluorapatite expressed as P 2 O 5 content has been tested in vitro in static and dynamic regime. The paper reports the complete results of bioactivity test of glass-ceramics in static regime. XRD, SEM, and microprobe analysis were used to characterise the sample as well as to detect the presence of new phase onto the surface. The bioactivity, as demonstrated by the formation of new apatite layer, depends on P 2 O 5 content. In static regime, the layer of hydroxyapatite develops by periodical deposition of spherical apatite bullet. In the dynamic test regime, the microstructure of apatite layer formed on the surface of sample is porous and grows as a result of continual reaction between the layer and fluid.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.