Abstract
This study investigates the potential use of the neuro-fuzzy (NF) approach to model the rutting prediction by the aid of repeated creep testing results for polypropylene modified asphalt mixtures. Marshall specimens, fabricated with M-03 type polypropylene fibers at optimum bitumen content have been tested in order to predict their rutting potential under different load values and loading patterns at 50°C. Throughout the testing phase, it has been clearly shown that the addition of polypropylene fibers results in improved Marshall stabilities and decrease in the flow values, providing an eminent increase of the service life of samples under repeated creep testing. The performance of the accuracy of proposed neuro-fuzzy model is observed to be quite satisfactory. In addition, to obtain the main effects plot, a wide range of detailed two and three dimensional parametric studies have been performed.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.