Abstract
The precipitation of β-NiAl phase in a high Ru-containing Ni-based single crystal superalloys was investigated. The β-NiAl phase is mainly distributed in the interdendritic region of the as-cast structure. And it was found parts of Ru elements were polarized in β-NiAl phase as the existence of strong bonds between Ru atoms and Al atoms. In addition, the solidification path of the experimental alloy passes through the region of the L → L1 + γ → L2 + γ + β-NiAl → L3 + γ + β-NiAl + precipitated γ′ → γ + β-NiAl + precipitated γ′ + γ/γ′ eutectics. It provides experimental data and theoretical guidance for the composition design of the novel Ru-containing high-generation Ni-SCs.