The precipitation of secondary Al3(Sc, Zr) particles in Al-Mg-Zn-Sc-Zr alloy during the two-stage homogenization has been studied by OM, SEM, and TEM. The results indicated that Al3(Sc, Zr) particles grew gradually with the first-stage homogenization temperature ranging from 380°C to 440°C. The first-stage homogenization temperature greatly affected the particle size of Al3(Sc, Zr). The lower the first-stage homogenization temperature was, the smaller the particle size of Al3(Sc, Zr) was. After the same second-stage homogenization treatment, the particles were coarsened, and the size was 15.2 nm, 15.9 nm, and 19.7 nm, respectively. Meanwhile, the Al3(Sc, Zr) particles exhibited a legume-like morphology and maintained a coherent relationship with the Al matrix after different homogenization treatments.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.