Abstract

In this article, the impact of long-term annealing on transformation of microstructure, in sand casting and die-casting Mg-5Al magnesium alloy was discussed. The Mg17Al12 phase of the diverse morphology is the basic strengthening phase in Mg-5Al alloys. After sand casting microstructure of Mg-5Al alloy consists of α-Mg solid solution with continuous and discontinuous precipitates of Mg17Al12 phase. After die-casting, the structure is characterized by significant grain refining of α-Mg solid solution, however Mg17Al12 phase, together with α-Mg solid solution, forms fully divorced eutectic. The Mg17Al12 phase undergo decomposition and coagulation at the temperature above 180°C and higher.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.