Abstract

In most of the reports on nanocrystal (NC) luminescent, the power depedence of luminescent intensity is studied using a continuous-wave laser with low power density, and the slopes of those different emission bands keep unchanged. In this paper, the up/down conversion of monodisperse Yb/Er: NaGdF4@Yb: NaGdF4@Yb: NaNdF4 NCs under the excitation of 800[Formula: see text]nm femtosecond laser was detected simultaneously by a home-built optical measurement setup. The power-dependent optical properties under the excitation of femtosecond laser are quite different from the normal situation, which is due to their high peak power and energy transfer processes: Nd[Formula: see text].

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.