The welding characteristics of a commercial wrought alloy with a nominal composition of Ni-29Co-28Cr-2.75Si were investigated. Gas tungsten arc weldments with filler metal matching the chemistry of the alloy were found to have limited room-temperature ductility in the as-welded condition. Since welding is the main fabrication method of this alloy, the welding and postweld heat treatment (PWHT) characteristics were examined to provide guidelines for fabrication in the field. Metallographic evaluation revealed that the weld metal was characterized by the distribution of a continuous eutectic phase consisting primarily of (Si,Ti)xNiy The continuous eutectic phase in the as-welded deposit, which caused poor ductility of the welds, was successfully reduced or removed with proper PWHT. The PWHT is necessary if cold forming of a weldment is required after welding or if adequate joint ductility is a design requirement. The recommended PWHT temperature is 1050 °C.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call